Ipe vs Miraúba
Tabebuia spp., lapacho group against Mouriri collocarpa. Every number below names the publication it came from.
| Property | Ipe | Miraúba |
|---|---|---|
| Janka hardness | 3,680 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 4,032 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 70.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 68.0 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 25,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 27,309 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.14 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,010 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 13,697 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 17.4%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.21USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 1.56LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Miraúba resists denting better. It tests 10% harder than Ipe.
- Ipe moves more evenly. Its tangential-to-radial ratio is 1.2 against 1.6, so it is the safer choice for a wide flat panel.
- Miraúba carries 8% more load in bending, which matters for a shelf or a rail.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.