Jarana vs Muirapixuna

Holopyxidium jarana against Chamaecrista scleroxylon = Cassia scleroxylon. Every number below names the publication it came from.

PropertyJaranaMuirapixuna
Janka hardness3,500 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)3,435 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)84.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture30,170 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)26,227 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.91 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength12,540 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)13,967 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)16.8%Chudnoff 1984, Tropical Timbers of the World (AH-607)11.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.34Chudnoff 1984, Tropical Timbers of the World (AH-607)2.28LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.
  • Jarana moves more evenly. Its tangential-to-radial ratio is 1.3 against 2.3, so it is the safer choice for a wide flat panel.
  • Jarana carries 15% more load in bending, which matters for a shelf or a rail.
  • Muirapixuna is the heavier of the two by 354 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.