PropertyJataipebaWamara
Janka hardness3,650 lbfLPF/SFB Madeiras Brasileiras3,692 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC63.7 lb/ft³LPF/SFB Madeiras Brasileiras70.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture24,614 lb/in²LPF/SFB Madeiras Brasileiras26,370 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.35 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras3.63 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,481 lb/in²LPF/SFB Madeiras Brasileiras15,440 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)14.5%LPF/SFB Madeiras Brasileiras11.2%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.75LPF/SFB Madeiras Brasileiras1.95Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Jataipeba moves more evenly. Its tangential-to-radial ratio is 1.7 against 1.9, so it is the safer choice for a wide flat panel.
  • Wamara is the heavier of the two by 101 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain