Wood Record

Kamassi vs Mecrusse

Goni orna kamassi against Androstachys johnsonii. Every number below names the publication it came from.

PropertyKamassiMecrusse
Janka hardness2,730 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,540 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,970 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)18,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.54 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Crushing strength10,530 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—11.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—1.07Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • Kamassi resists denting better. It tests 7% harder than Mecrusse.
  • Kamassi carries 12% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons