Kamassi vs Missanda
Goni orna kamassi against Erythrophleum ivorense. Every number below names the publication it came from.
| Property | Kamassi | Missanda |
|---|---|---|
| Janka hardness | 2,730 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of rupture | 20,970 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 23,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.54 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.24 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 10,530 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 14,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | — | — |
| Tangential / radial ratio(lower is better) | — | — |
What the numbers mean
- Missanda resists denting better. It tests 7% harder than Kamassi.
- Missanda carries 12% more load in bending, which matters for a shelf or a rail.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.