| Property | Kaneelhart | Sucupira |
|---|---|---|
| Janka hardness | 2,900 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2,903 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 59.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 29,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 23,663 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 4.06 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2.33 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 17,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 13,536 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 12.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 12.3%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.46USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 1.64LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Kaneelhart carries 26% more load in bending, which matters for a shelf or a rail.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.