Leche Perra vs Maçarandubarana
Helicostylis tomentosa against Chrysophyllum prieurii. Every number below names the publication it came from.
| Property | Leche Perra | Maçarandubarana |
|---|---|---|
| Janka hardness | 2,700 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,725 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 55.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 61.8 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 22,800 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 25,232 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.86 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 10,810 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 14.6%Chudnoff 1984, Tropical Timbers of the World (AH-607) | 20.3%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.70Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.69LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Maçarandubarana carries 11% more load in bending, which matters for a shelf or a rail.
- Maçarandubarana is the heavier of the two by 109 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.