Maçaranduba vs Maçaranduba
Manilkara sp. against Manilkara huberi. Every number below names the publication it came from.
| Property | Maçaranduba | Maçaranduba |
|---|---|---|
| Janka hardness | 3,228 lbfLPF/SFB Madeiras Brasileiras | 3,047 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 66.8 lb/ft³LPF/SFB Madeiras Brasileiras | 66.8 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 24,593 lb/in²LPF/SFB Madeiras Brasileiras | 25,560 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.02 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.47 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,961 lb/in²LPF/SFB Madeiras Brasileiras | 15,774 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 16.4%LPF/SFB Madeiras Brasileiras | 16.4%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.40LPF/SFB Madeiras Brasileiras | 1.31LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Maçaranduba resists denting better. It tests 6% harder than Maçaranduba.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.