Macawood vs Pracuúba-da-terra-firme
Platymiscium spp. against Trichilia lecointei. Every number below names the publication it came from.
| Property | Macawood | Pracuúba-da-terra-firme |
|---|---|---|
| Janka hardness | 3,150 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 3,159 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 64.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 73.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 27,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 22,871 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.20 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 16,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b | 12,531 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 6.5%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 13.2%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.30USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4 | 1.86LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Macawood moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.9, so it is the safer choice for a wide flat panel.
- Macawood carries 21% more load in bending, which matters for a shelf or a rail.
- Pracuúba-da-terra-firme is the heavier of the two by 151 kg/m³, which a reader building a door or a case should weigh.
Sources
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
- USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.