Wood Record

Manbarklak vs Marishballi

Eschweilera spp. against Lincania spp.. Every number below names the publication it came from.

PropertyManbarklakMarishballi
Janka hardness3,480 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3,570 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC46.2 lb/ft³LPF/SFB Madeiras Brasileiras62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture26,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b27,700 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity3.14 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3.34 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength11,210 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b13,390 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)15.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-417.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)1.78USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.56USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

What the numbers mean

  • The two match on hardness, within 3%. Choose on movement or on appearance instead.
  • Marishballi moves more evenly. Its tangential-to-radial ratio is 1.6 against 1.8, so it is the safer choice for a wide flat panel.
  • Marishballi is the heavier of the two by 253 kg/m³, which a reader building a door or a case should weigh.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons