Wood Record

Manbarklak vs Rosadinho

Eschweilera spp. against Peltogyne paniculata. Every number below names the publication it came from.

PropertyManbarklakRosadinho
Janka hardness3,480 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b3,386 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC46.2 lb/ft³LPF/SFB Madeiras Brasileiras64.3 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture26,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b27,138 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity3.14 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,210 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b13,129 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.9%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-412.7%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.78USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.59LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 3%. Choose on movement or on appearance instead.
  • Rosadinho is the heavier of the two by 290 kg/m³, which a reader building a door or a case should weigh.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons