| Property | Maria-preta | Muirapixuna |
|---|---|---|
| Janka hardness | 3,331 lbfLPF/SFB Madeiras Brasileiras | 3,435 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 60.6 lb/ft³LPF/SFB Madeiras Brasileiras | 84.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 22,714 lb/in²LPF/SFB Madeiras Brasileiras | 26,227 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.35 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.38 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 12,688 lb/in²LPF/SFB Madeiras Brasileiras | 13,967 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.7%LPF/SFB Madeiras Brasileiras | 11.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.43LPF/SFB Madeiras Brasileiras | 2.28LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 3%. Choose on movement or on appearance instead.
- Maria-preta moves more evenly. Its tangential-to-radial ratio is 1.4 against 2.3, so it is the safer choice for a wide flat panel.
- Muirapixuna carries 15% more load in bending, which matters for a shelf or a rail.
- Muirapixuna is the heavier of the two by 377 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.