Matamatá vs Matamatá
Eschweilera grandiflora = Eschweilera cf fracta against Eschweilera pedicellata = Eschweilera longipes. Every number below names the publication it came from.
| Property | Matamatá | Matamatá |
|---|---|---|
| Janka hardness | 1,995 lbfLPF/SFB Madeiras Brasileiras | 2,410 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 53.1 lb/ft³LPF/SFB Madeiras Brasileiras | 61.2 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 19,728 lb/in²LPF/SFB Madeiras Brasileiras | 19,444 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.10 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.29 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 9,757 lb/in²LPF/SFB Madeiras Brasileiras | 9,673 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 14.9%LPF/SFB Madeiras Brasileiras | 14.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.74LPF/SFB Madeiras Brasileiras | 1.72LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Matamatá resists denting better. It tests 21% harder than Matamatá.
- Matamatá is the heavier of the two by 130 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain