| Property | Matamatá | Matamatá / sapucaia-amargosa |
|---|---|---|
| Janka hardness | 1,995 lbfLPF/SFB Madeiras Brasileiras | 2,341 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 53.1 lb/ft³LPF/SFB Madeiras Brasileiras | 60.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 19,728 lb/in²LPF/SFB Madeiras Brasileiras | 20,453 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.10 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.13 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 9,757 lb/in²LPF/SFB Madeiras Brasileiras | 10,055 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 14.9%LPF/SFB Madeiras Brasileiras | 15.3%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.74LPF/SFB Madeiras Brasileiras | 2.10LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Matamatá / sapucaia-amargosa resists denting better. It tests 17% harder than Matamatá.
- Matamatá moves more evenly. Its tangential-to-radial ratio is 1.7 against 2.1, so it is the safer choice for a wide flat panel.
- Matamatá / sapucaia-amargosa is the heavier of the two by 118 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain