Matamatá / sapucaia-amargosa vs Uxi
Lecythis idatimon against Endopleura uchi. Every number below names the publication it came from.
| Property | Matamatá / sapucaia-amargosa | Uxi |
|---|---|---|
| Janka hardness | 2,341 lbfLPF/SFB Madeiras Brasileiras | 2,335 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 60.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 20,453 lb/in²LPF/SFB Madeiras Brasileiras | 22,288 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.13 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 10,055 lb/in²LPF/SFB Madeiras Brasileiras | 10,852 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.3%LPF/SFB Madeiras Brasileiras | 15.6%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 2.10LPF/SFB Madeiras Brasileiras | 1.50LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 0%. Choose on movement or on appearance instead.
- Uxi moves more evenly. Its tangential-to-radial ratio is 1.5 against 2.1, so it is the safer choice for a wide flat panel.
- Uxi carries 9% more load in bending, which matters for a shelf or a rail.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.