Wood Record

Matamatá vs Matamatá

Eschweilera coriacea against Eschweilera pedicellata = Eschweilera longipes. Every number below names the publication it came from.

PropertyMatamatáMatamatá
Janka hardness2,467 lbfLPF/SFB Madeiras Brasileiras2,410 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC56.2 lb/ft³LPF/SFB Madeiras Brasileiras61.2 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture19,002 lb/in²LPF/SFB Madeiras Brasileiras19,444 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.11 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.29 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength9,181 lb/in²LPF/SFB Madeiras Brasileiras9,673 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)16.0%LPF/SFB Madeiras Brasileiras14.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.71LPF/SFB Madeiras Brasileiras1.72LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.
  • Matamatá is the heavier of the two by 80 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons