| Property | Matamatá | Matamatá / sapucaia-amargosa |
|---|---|---|
| Janka hardness | 2,467 lbfLPF/SFB Madeiras Brasileiras | 2,341 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 56.2 lb/ft³LPF/SFB Madeiras Brasileiras | 60.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 19,002 lb/in²LPF/SFB Madeiras Brasileiras | 20,453 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.11 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.13 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 9,181 lb/in²LPF/SFB Madeiras Brasileiras | 10,055 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 16.0%LPF/SFB Madeiras Brasileiras | 15.3%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.71LPF/SFB Madeiras Brasileiras | 2.10LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Matamatá resists denting better. It tests 5% harder than Matamatá / sapucaia-amargosa.
- Matamatá moves more evenly. Its tangential-to-radial ratio is 1.7 against 2.1, so it is the safer choice for a wide flat panel.
- Matamatá / sapucaia-amargosa carries 8% more load in bending, which matters for a shelf or a rail.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain