Miraúba vs Urucurana
Mouriri collocarpa against Sloanea nitida. Every number below names the publication it came from.
| Property | Miraúba | Urucurana |
|---|---|---|
| Janka hardness | 4,032 lbfLPF/SFB Madeiras Brasileiras | 4,057 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 68.0 lb/ft³LPF/SFB Madeiras Brasileiras | 67.4 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 27,309 lb/in²LPF/SFB Madeiras Brasileiras | 24,877 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,697 lb/in²LPF/SFB Madeiras Brasileiras | 13,854 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 17.4%LPF/SFB Madeiras Brasileiras | 18.6%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.56LPF/SFB Madeiras Brasileiras | 2.13LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Miraúba moves more evenly. Its tangential-to-radial ratio is 1.6 against 2.1, so it is the safer choice for a wide flat panel.
- Miraúba carries 10% more load in bending, which matters for a shelf or a rail.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.