Miraúba vs Urucurana
Mouriri collocarpa against Sloanea sp.. Every number below names the publication it came from.
| Property | Miraúba | Urucurana |
|---|---|---|
| Janka hardness | 4,032 lbfLPF/SFB Madeiras Brasileiras | 4,206 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 68.0 lb/ft³LPF/SFB Madeiras Brasileiras | 59.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 27,309 lb/in²LPF/SFB Madeiras Brasileiras | 21,747 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.49 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.32 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,697 lb/in²LPF/SFB Madeiras Brasileiras | 11,137 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 17.4%LPF/SFB Madeiras Brasileiras | 15.5%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.56LPF/SFB Madeiras Brasileiras | 1.55LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 4%. Choose on movement or on appearance instead.
- Miraúba carries 26% more load in bending, which matters for a shelf or a rail.
- Miraúba is the heavier of the two by 130 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.