Missanda vs Okan
Erythrophleum ivorense against Cylicodiscus gabunensis. Every number below names the publication it came from.
| Property | Missanda | Okan |
|---|---|---|
| Janka hardness | 2,930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,780 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) |
| Density at 12% MC | 56.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 23,500 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 20,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Modulus of elasticity | 2.24 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.33 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Crushing strength | 14,100 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 12,380 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Volumetric shrinkage(lower is better) | — | 12.6%Chudnoff 1984, Tropical Timbers of the World (AH-607) |
| Tangential / radial ratio(lower is better) | — | 1.47Chudnoff 1984, Tropical Timbers of the World (AH-607) |
What the numbers mean
- Missanda resists denting better. It tests 5% harder than Okan.
- Missanda carries 16% more load in bending, which matters for a shelf or a rail.
- Okan is the heavier of the two by 130 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.