Wood Record

Mora vs Uxi

Mora spp. against Endopleura uchi. Every number below names the publication it came from.

PropertyMoraUxi
Janka hardness2,300 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,335 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC62.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)62.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture22,100 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b22,288 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.96 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,840 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b10,852 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)18.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-415.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.42USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.50LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 2%. Choose on movement or on appearance instead.

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons