Brachylaena hutchinsii against Buchenavia cf viridiflora. Every number below names the publication it came from.

PropertyMuhuhuTaniboca
Janka hardness2,190 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,191 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)54.9 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture16,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)17,110 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.46 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.89 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength10,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,587 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)—11.2%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)—1.65LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 0%. Choose on movement or on appearance instead.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons