Wood Record

Ohia vs Pyinkado

Metrosideros collina subsp. polymorpha against Xylia xylocarpa. Every number below names the publication it came from.

PropertyOhiaPyinkado
Janka hardness2,090 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,248 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC57.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)61.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture18,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)21,200 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.37 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Crushing strength8,900 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)—11.1%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)—2.03Chudnoff 1984, Tropical Timbers of the World (AH-607)

What the numbers mean

  • Pyinkado resists denting better. It tests 8% harder than Ohia.
  • Pyinkado carries 16% more load in bending, which matters for a shelf or a rail.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons