PropertyOkanRhodesian-Teak
Janka hardness2,780 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)2,990 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-956.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture20,300 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)12,220 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity2.33 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.23 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength12,380 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)9,600 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)12.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)—
Tangential / radial ratio(lower is better)1.47Chudnoff 1984, Tropical Timbers of the World (AH-607)—

What the numbers mean

  • Rhodesian-Teak resists denting better. It tests 8% harder than Okan.
  • Okan carries 66% more load in bending, which matters for a shelf or a rail.
  • Okan is the heavier of the two by 130 kg/m³, which a reader building a door or a case should weigh.

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.