Pau-amarelo vs Taniboca
Euxylophora paraensis against Buchenavia cf viridiflora. Every number below names the publication it came from.
| Property | Pau-amarelo | Taniboca |
|---|---|---|
| Janka hardness | 2,168 lbfLPF/SFB Madeiras Brasileiras | 2,191 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 50.6 lb/ft³LPF/SFB Madeiras Brasileiras | 54.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 17,566 lb/in²LPF/SFB Madeiras Brasileiras | 17,110 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 1.92 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 1.89 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 10,092 lb/in²LPF/SFB Madeiras Brasileiras | 9,587 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 11.1%LPF/SFB Madeiras Brasileiras | 11.2%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.36LPF/SFB Madeiras Brasileiras | 1.65LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 1%. Choose on movement or on appearance instead.
- Pau-amarelo moves more evenly. Its tangential-to-radial ratio is 1.4 against 1.7, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.