Pau-branco vs Urucurana
Drypetes variabilis against Swartzia recurva. Every number below names the publication it came from.
| Property | Pau-branco | Urucurana |
|---|---|---|
| Janka hardness | 2,518 lbfLPF/SFB Madeiras Brasileiras | 2,469 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 55.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 57.4 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 20,865 lb/in²LPF/SFB Madeiras Brasileiras | 22,345 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.30 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.42 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 10,511 lb/in²LPF/SFB Madeiras Brasileiras | 10,596 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.9%LPF/SFB Madeiras Brasileiras | 15.0%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.95LPF/SFB Madeiras Brasileiras | 1.37LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 2%. Choose on movement or on appearance instead.
- Urucurana moves more evenly. Its tangential-to-radial ratio is 1.4 against 1.9, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.