Sapucaia / sapucaia-vermelha vs Sucupira
Lecythis pisonis subsp. usitata against Bowdichia nitida. Every number below names the publication it came from.
| Property | Sapucaia / sapucaia-vermelha | Sucupira |
|---|---|---|
| Janka hardness | 2,831 lbfLPF/SFB Madeiras Brasileiras | 2,903 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 67.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 59.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 21,747 lb/in²LPF/SFB Madeiras Brasileiras | 23,663 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.33 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 10,185 lb/in²LPF/SFB Madeiras Brasileiras | 13,536 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.9%LPF/SFB Madeiras Brasileiras | 12.3%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.43LPF/SFB Madeiras Brasileiras | 1.64LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 3%. Choose on movement or on appearance instead.
- Sapucaia / sapucaia-vermelha moves more evenly. Its tangential-to-radial ratio is 1.4 against 1.6, so it is the safer choice for a wide flat panel.
- Sucupira carries 9% more load in bending, which matters for a shelf or a rail.
- Sapucaia / sapucaia-vermelha is the heavier of the two by 125 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.