Sapucaia vs Sapucaia / sapucaia-vermelha
Lecythis spp. against Lecythis pisonis subsp. usitata. Every number below names the publication it came from.
| Property | Sapucaia | Sapucaia / sapucaia-vermelha |
|---|---|---|
| Janka hardness | 3,100 lbfChudnoff 1984, Tropical Timbers of the World (AH-607) | 2,831 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 58.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607) | 67.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 27,540 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 21,747 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 3.38 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 2.15 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,280 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607) | 10,185 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 13.4%Chudnoff 1984, Tropical Timbers of the World (AH-607) | 13.9%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.27Chudnoff 1984, Tropical Timbers of the World (AH-607) | 1.43LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Sapucaia resists denting better. It tests 10% harder than Sapucaia / sapucaia-vermelha.
- Sapucaia carries 27% more load in bending, which matters for a shelf or a rail.
- Sapucaia / sapucaia-vermelha is the heavier of the two by 156 kg/m³, which a reader building a door or a case should weigh.
Sources
- Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
- LPF/SFB Madeiras BrasileirasCC BY 4.0
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.