Taniboca vs Tanimbuca
Buchenavia cf viridiflora against Terminalia amazonia. Every number below names the publication it came from.
| Property | Taniboca | Tanimbuca |
|---|---|---|
| Janka hardness | 2,191 lbfLPF/SFB Madeiras Brasileiras | 2,235 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 54.9 lb/ft³LPF/SFB Madeiras Brasileiras | 64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 |
| Modulus of rupture | 17,110 lb/in²LPF/SFB Madeiras Brasileiras | 21,178 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 1.89 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.03 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 9,587 lb/in²LPF/SFB Madeiras Brasileiras | 11,307 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 11.2%LPF/SFB Madeiras Brasileiras | 12.8%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.65LPF/SFB Madeiras Brasileiras | 1.50LPF/SFB Madeiras Brasileiras |
What the numbers mean
- The two match on hardness, within 2%. Choose on movement or on appearance instead.
- Tanimbuca carries 24% more load in bending, which matters for a shelf or a rail.
- Tanimbuca is the heavier of the two by 147 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.