Wood Record

Tanimbuca vs Tanimbuca

Buchenavia tetraphylla = Buchenavia capitata against Terminalia amazonia. Every number below names the publication it came from.

PropertyTanimbucaTanimbuca
Janka hardness1,640 lbfLPF/SFB Madeiras Brasileiras2,235 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC52.4 lb/ft³LPF/SFB Madeiras Brasileiras64.1 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture15,618 lb/in²LPF/SFB Madeiras Brasileiras21,178 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity1.81 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.03 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength8,605 lb/in²LPF/SFB Madeiras Brasileiras11,307 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)16.7%LPF/SFB Madeiras Brasileiras12.8%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.97LPF/SFB Madeiras Brasileiras1.50LPF/SFB Madeiras Brasileiras

What the numbers mean

  • Tanimbuca resists denting better. It tests 36% harder than Tanimbuca.
  • Tanimbuca moves more evenly. Its tangential-to-radial ratio is 1.5 against 2.0, so it is the safer choice for a wide flat panel.
  • Tanimbuca carries 36% more load in bending, which matters for a shelf or a rail.
  • Tanimbuca is the heavier of the two by 187 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons