Wood Record

Tuturubá vs Uxirana

Pouteria oblanceolata against Vantanea parviflora. Every number below names the publication it came from.

PropertyTuturubáUxirana
Janka hardness2,923 lbfLPF/SFB Madeiras Brasileiras2,948 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC59.9 lb/ft³LPF/SFB Madeiras Brasileiras69.7 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture22,217 lb/in²LPF/SFB Madeiras Brasileiras24,635 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.55 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength11,293 lb/in²LPF/SFB Madeiras Brasileiras12,531 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.8%LPF/SFB Madeiras Brasileiras17.6%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.71LPF/SFB Madeiras Brasileiras1.26LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 1%. Choose on movement or on appearance instead.
  • Uxirana moves more evenly. Its tangential-to-radial ratio is 1.3 against 1.7, so it is the safer choice for a wide flat panel.
  • Uxirana carries 11% more load in bending, which matters for a shelf or a rail.
  • Uxirana is the heavier of the two by 156 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons