Tuturubá vs Tuturubá
Pouteria gongrijpii = Franchetella gongrijpii against Pouteria oblanceolata. Every number below names the publication it came from.
| Property | Tuturubá | Tuturubá |
|---|---|---|
| Janka hardness | 2,396 lbfLPF/SFB Madeiras Brasileiras | 2,923 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 56.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9 | 59.9 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 20,951 lb/in²LPF/SFB Madeiras Brasileiras | 22,217 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 10,952 lb/in²LPF/SFB Madeiras Brasileiras | 11,293 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.0%LPF/SFB Madeiras Brasileiras | 13.8%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 2.24LPF/SFB Madeiras Brasileiras | 1.71LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Tuturubá resists denting better. It tests 22% harder than Tuturubá.
- Tuturubá moves more evenly. Its tangential-to-radial ratio is 1.7 against 2.2, so it is the safer choice for a wide flat panel.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.