Urucurana vs Urucurana
Sloanea sp. against Swartzia recurva. Every number below names the publication it came from.
| Property | Urucurana | Urucurana |
|---|---|---|
| Janka hardness | 4,206 lbfLPF/SFB Madeiras Brasileiras | 2,469 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 59.9 lb/ft³LPF/SFB Madeiras Brasileiras | 57.4 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 21,747 lb/in²LPF/SFB Madeiras Brasileiras | 22,345 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.32 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.42 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 11,137 lb/in²LPF/SFB Madeiras Brasileiras | 10,596 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 15.5%LPF/SFB Madeiras Brasileiras | 15.0%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 1.55LPF/SFB Madeiras Brasileiras | 1.37LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Urucurana resists denting better. It tests 70% harder than Urucurana.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.