Wood Record

Urucurana vs Urucurana

Sloanea nitida against Sloanea sp.. Every number below names the publication it came from.

PropertyUrucuranaUrucurana
Janka hardness4,057 lbfLPF/SFB Madeiras Brasileiras4,206 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC67.4 lb/ft³LPF/SFB Madeiras Brasileiras59.9 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture24,877 lb/in²LPF/SFB Madeiras Brasileiras21,747 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.32 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength13,854 lb/in²LPF/SFB Madeiras Brasileiras11,137 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)18.6%LPF/SFB Madeiras Brasileiras15.5%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.13LPF/SFB Madeiras Brasileiras1.55LPF/SFB Madeiras Brasileiras

What the numbers mean

  • The two match on hardness, within 4%. Choose on movement or on appearance instead.
  • Urucurana moves more evenly. Its tangential-to-radial ratio is 1.5 against 2.1, so it is the safer choice for a wide flat panel.
  • Urucurana carries 14% more load in bending, which matters for a shelf or a rail.
  • Urucurana is the heavier of the two by 120 kg/m³, which a reader building a door or a case should weigh.

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons