Urucurana vs Urucurana
Sloanea nitida against Swartzia recurva. Every number below names the publication it came from.
| Property | Urucurana | Urucurana |
|---|---|---|
| Janka hardness | 4,057 lbfLPF/SFB Madeiras Brasileiras | 2,469 lbfLPF/SFB Madeiras Brasileiras |
| Density at 12% MC | 67.4 lb/ft³LPF/SFB Madeiras Brasileiras | 57.4 lb/ft³LPF/SFB Madeiras Brasileiras |
| Modulus of rupture | 24,877 lb/in²LPF/SFB Madeiras Brasileiras | 22,345 lb/in²LPF/SFB Madeiras Brasileiras |
| Modulus of elasticity | 2.57 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras | 2.42 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras |
| Crushing strength | 13,854 lb/in²LPF/SFB Madeiras Brasileiras | 10,596 lb/in²LPF/SFB Madeiras Brasileiras |
| Volumetric shrinkage(lower is better) | 18.6%LPF/SFB Madeiras Brasileiras | 15.0%LPF/SFB Madeiras Brasileiras |
| Tangential / radial ratio(lower is better) | 2.13LPF/SFB Madeiras Brasileiras | 1.37LPF/SFB Madeiras Brasileiras |
What the numbers mean
- Urucurana resists denting better. It tests 64% harder than Urucurana.
- Urucurana moves more evenly. Its tangential-to-radial ratio is 1.4 against 2.1, so it is the safer choice for a wide flat panel.
- Urucurana carries 11% more load in bending, which matters for a shelf or a rail.
- Urucurana is the heavier of the two by 160 kg/m³, which a reader building a door or a case should weigh.
Sources
- LPF/SFB Madeiras BrasileirasCC BY 4.0
- USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.