family
Acanthaceae
The family Acanthaceae supplies 3 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Avicennia marinaAvicennia marina | 1,658 lbf* | 48.9 lb/ft³ |
| BiutAvicennia alba | 1,725 lbf* | 49.9 lb/ft³ |
| Black mangroveAvicennia germinans | 2,139 lbf* | 55.1 lb/ft³ |