family
Altingiaceae
The family Altingiaceae supplies 2 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Oriental sweetgumLiquidambar orientalis | 791 lbf* | 34.7 lb/ft³ |
| SweetgumLiquidambar styraciflua | 850 lbf | 36.3 lb/ft³ |