| Wood | Janka | Density |
|---|---|---|
| African sumacRhus lancea | 818 lbf* | 35.2 lb/ft³ |
| CajáSpondias mombin = Spondias lutea | 359 lbf | 28.1 lb/ft³ |
| CajuaçuAnacardium giganteum | 505 lbf | 30.6 lb/ft³ |
| CajuaçuAnacardium occidentale = Anacardium microcarpum | 591 lbf | 28.7 lb/ft³ |
| CajuaçuAnacardium parvifolium | 657 lbf | 31.5 lb/ft³ |
| CajuaçuAnacardium spruceanum | 560 lbf | 31.5 lb/ft³ |
| CarrascoComocladia glabra | 2,607 lbf* | 60.4 lb/ft³ |
| ChechenMetopium brownei | 1,923 lbf* | 52.4 lb/ft³ |
| Chinese pistachePistacia chinensis | 2,287 lbf* | 56.9 lb/ft³ |
| EspaveAnacardium excelsum | 470 lbf | 30.0 lb/ft³ |
| European smoketreeCotinus coggygria | 1,475 lbf* | 46.4 lb/ft³ |
| Florida poisontreeMetopium toxiferum | 915 lbf* | 37.1 lb/ft³ |
| Goncalo alvesAstronium graveolens | 2,160 lbf | 67.7 lb/ft³ |
| KanitMangifera minor | 1,255 lbf* | 43.0 lb/ft³ |
| KelelacharmCampnosperma brevipetiolatum | 423 lbf* | 26.0 lb/ft³ |
| MangoMangifera spp. | 1,000 lbf | 40.0 lb/ft³ |
| MangoMangifera indica | 1,103 lbf* | 40.5 lb/ft³ |
| MerpauhSwintonia spp. | 1,075 lbf | 46.0 lb/ft³ |
| MuiracatiaraAstronium ulei | 1,684 lbf | 55.9 lb/ft³ |
| Muiracatiara-rajadaAstronium lecointei | 2,051 lbf | 61.3 lb/ft³ |
| PaldaoDracontomelum spp. | 980 lbf | 38.0 lb/ft³ |
| Peruvian peppertreeSchinus molle | 1,203 lbf* | 42.1 lb/ft³ |
| Poison ashComocladia dodonaea | 3,749 lbf* | 71.5 lb/ft³ |
| Poison sumacToxicodendron vernix | 714 lbf* | 33.1 lb/ft³ |
| Prairie sumacRhus lanceolata | 679 lbf* | 32.3 lb/ft³ |
| Purple mombinSpondias purpurea | 423 lbf* | 26.0 lb/ft³ |
| QuebrachoSchinopsis spp. | 5,180 lbf* | 75.0 lb/ft³ |
| RangguKoordersiodendron pinnatum | 1,860 lbf | 52.0 lb/ft³ |
| RengasGluta spp. | 1,720 lbf | 48.5 lb/ft³ |
| Saipan mangoMangifera odorata | 1,054 lbf* | 39.6 lb/ft³ |
| SajoCampnosperma panamensis | 425 lbf | 25.0 lb/ft³ |
| SmoketreeCotinus obovatus | 1,309 lbf* | 43.8 lb/ft³ |
| South African wild plumHarpephyllum caffrum | 641 lbf* | 31.5 lb/ft³ |
| Spondias dulcisSpondias dulcis | 395 lbf* | 25.1 lb/ft³ |
| Staghorn sumacRhus typhina | 818 lbf* | 35.2 lb/ft³ |
| TatapiriricaTapirira guianensis | 891 lbf | 38.0 lb/ft³ |
| TavaiRhus taitensis | 714 lbf* | 33.1 lb/ft³ |
| TitmelSpondias pinnata | 321 lbf* | 22.8 lb/ft³ |
| Winged sumacRhus copallinum | 818 lbf* | 35.2 lb/ft³ |