family
Annonaceae
The family Annonaceae supplies 20 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
8 of 20 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Annona cherimolaAnnona cherimola | 1,255 lbf* | 43.0 lb/ft³ |
| CanangaCanangium odoratum | 330 lbf | 23.0 lb/ft³ |
| Custard appleAnnona reticulata | 791 lbf* | 34.7 lb/ft³ |
| EmbiraAnnona exsucca = Rollinia exsucca | 864 lbf | 39.6 lb/ft³ |
| Embira-brancaXylopia nitida | 1,118 lbf | 43.0 lb/ft³ |
| Embira-pretaGuatteria olivacea | 883 lbf | 53.1 lb/ft³ |
| Embira-pretaDiclinanona calycina | 888 lbf | 35.5 lb/ft³ |
| Embira-pretaGuatteria procera | 1,468 lbf | 50.7 lb/ft³ |
| Enbira-pretaOnychopetalum amazonicum | 1,396 lbf | 46.8 lb/ft³ |
| HayaOxandra laurifolia | 1,725 lbf* | 49.9 lb/ft³ |
| Haya blancaGuatteria caribaea | 1,203 lbf* | 42.1 lb/ft³ |
| Haya mingaGuatteria blainii | 1,598 lbf* | 48.1 lb/ft³ |
| Ilang-ilangCananga odorata | 509 lbf* | 28.2 lb/ft³ |
| Mountain soursopAnnona montana | 753 lbf* | 33.9 lb/ft³ |
| PawpawAsimina triloba | 509 lbf* | 28.2 lb/ft³ |
| Pond-appleAnnona glabra | 753 lbf* | 33.9 lb/ft³ |
| Smallflower pawpawAsimina parviflora | 1,054 lbf* | 39.6 lb/ft³ |
| SoursopAnnona muricata | 479 lbf* | 27.5 lb/ft³ |
| Sugar appleAnnona squamosa | 1,419 lbf* | 45.5 lb/ft³ |
| West Indian LancewoodOxandra lanceolata | 2,830 lbf | 62.0 lb/ft³ |