family
Apocynaceae
The family Apocynaceae supplies 24 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
9 of 24 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AlstoniaAlstonia congensis | 410 lbf | 25.0 lb/ft³ |
| Amapa amargosoParahancornia fasciculata = Parahancornia amapa | 789 lbf | 35.0 lb/ft³ |
| AraracangaAspidosperma desmanthum | 1,757 lbf | 51.2 lb/ft³ |
| ChiuteCerbera odollam | 395 lbf* | 25.1 lb/ft³ |
| Cow TreeCouma macrocarpa | 980 lbf | 38.0 lb/ft³ |
| DeviltreeAlstonia macrophylla | 1,538 lbf* | 47.3 lb/ft³ |
| EmeridechCerbera floribunda | 753 lbf* | 33.9 lb/ft³ |
| Gogó-de-guaribaRauvolfia paraensis | 1,203 lbf* | 44.3 lb/ft³ |
| JelutongDyera costulata | 390 lbf | 28.0 lb/ft³ |
| KamassiGoni orna kamassi | 2,730 lbf | 58.0 lb/ft³ |
| LevaCerbera manghas | 451 lbf* | 26.7 lb/ft³ |
| MilkwoodTabernaemontana citrifolia | 832 lbf* | 35.5 lb/ft³ |
| NosegaytreePlumeria alba | 1,725 lbf* | 49.9 lb/ft³ |
| OleanderNerium oleander | 832 lbf* | 35.5 lb/ft³ |
| PerobaAspidosperma macrocarpon | 1,852 lbf | 48.7 lb/ft³ |
| Peroba rosaAspidosperma spp., peroba group | 1,730 lbf | 51.5 lb/ft³ |
| Poison devil's-pepperRauvolfia vomitoria | 1,007 lbf* | 38.8 lb/ft³ |
| PulaiAlstonia spp. | 460 lbf | 28.0 lb/ft³ |
| PuluTabernaemontana pandacaqui | 1,419 lbf* | 45.5 lb/ft³ |
| RoostertreeCalotropis procera | 369 lbf* | 24.3 lb/ft³ |
| SilkrubberFuntumia elastica | 573 lbf* | 29.8 lb/ft³ |
| Singapore graveyard flowerPlumeria obtusa | 753 lbf* | 33.9 lb/ft³ |
| Tabernaemontana aurantiacaTabernaemontana aurantiaca | 1,152 lbf* | 41.3 lb/ft³ |
| TempletreePlumeria rubra | 1,007 lbf* | 38.8 lb/ft³ |