family
Aquifoliaceae
The family Aquifoliaceae supplies 9 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 9 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| American hollyIlex opaca | 960 lbf* | 38.0 lb/ft³ |
| CatberryIlex mucronata | 960 lbf* | 38.0 lb/ft³ |
| DahoonIlex cassine | 1,152 lbf* | 41.3 lb/ft³ |
| English hollyIlex aquifolium | 1,852 lbf* | 51.5 lb/ft³ |
| GongolinIlex sideroxyloides | 1,788 lbf* | 50.7 lb/ft³ |
| Hawaii hollyIlex anomala | 791 lbf* | 34.7 lb/ft³ |
| MateIlex paraguariensis | 960 lbf* | 38.0 lb/ft³ |
| Puerto Rico hollyIlex nitida | 2,139 lbf* | 55.1 lb/ft³ |
| YauponIlex vomitoria | 1,054 lbf* | 39.6 lb/ft³ |