Wood Record

family

Araliaceae

The family Araliaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

1 of 5 carry a published Janka test.

WoodJankaDensity
BngeiPolyscias nodosa479 lbf*27.5 lb/ft³
Devil's walkingstickAralia spinosa641 lbf*31.5 lb/ft³
Japanese angelica treeAralia elata395 lbf*25.1 lb/ft³
MorototóSchefflera morototoni789 lbf30.7 lb/ft³
OlapalapaCheirodendron trigynum1,054 lbf*39.6 lb/ft³