Araucariaceae

The family Araucariaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

1 of 6 carry a published Janka test.

WoodJankaDensity
KauriAgathis australis960 lbf*38.0 lb/ft³
Monkeypuzzle treeAraucaria araucana766 lbf*38.0 lb/ft³
New Caledonia pineAraucaria columnaris554 lbf*30.7 lb/ft³
Parana pineAraucaria angustifolia645 lbf*33.9 lb/ft³
Parana-pineAraucaria augustifolia780 lbf34.7 lb/ft³
Queensland kauriAgathis robusta573 lbf*29.8 lb/ft³