family
Arecaceae
The family Arecaceae supplies 13 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 13 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Alexandra palmArchontophoenix alexandrae | 2,779 lbf* | 62.2 lb/ft³ |
| Bangalow palmArchontophoenix cunninghamiana | 2,530 lbf* | 59.6 lb/ft³ |
| BetelnutAreca catechu | 875 lbf* | 36.3 lb/ft³ |
| Cabbage palmettoSabal palmetto | 641 lbf* | 31.5 lb/ft³ |
| California fan palmWashingtonia filifera | 832 lbf* | 35.5 lb/ft³ |
| Chinese windmill palmTrachycarpus fortunei | 276 lbf* | 21.2 lb/ft³ |
| Coconut palmCocos nucifera | 1,007 lbf* | 38.8 lb/ft³ |
| Dwarf palmettoSabal minor | 1,054 lbf* | 39.6 lb/ft³ |
| Fountain palmLivistona chinensis | 216 lbf* | 19.0 lb/ft³ |
| Oil nut palmElaeis guineensis | 1,054 lbf* | 39.6 lb/ft³ |
| Prestoea acuminataPrestoea acuminata | 395 lbf* | 25.1 lb/ft³ |
| Puerto Rico royal palmRoystonea borinquena | 2,287 lbf* | 56.9 lb/ft³ |
| Queen palmSyagrus romanzoffiana | 1,788 lbf* | 50.7 lb/ft³ |