Wood Record

family

Asparagaceae

The family Asparagaceae supplies 4 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 4 carry a published Janka test.

WoodJankaDensity
Eve's needleYucca faxoniana1,054 lbf*39.6 lb/ft³
Fragrant dracaenaDracaena fragrans679 lbf*32.3 lb/ft³
Joshua treeYucca brevifolia679 lbf*32.3 lb/ft³
Song of IndiaDracaena reflexa714 lbf*33.1 lb/ft³