Wood Record

family

Betulaceae

The family Betulaceae supplies 27 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

4 of 27 carry a published Janka test.

WoodJankaDensity
Alaska paper birchBetula neoalaskana——
American hornbeamCarpinus caroliniana1,363 lbf*44.7 lb/ft³
Arizona alderAlnus oblongifolia479 lbf*27.5 lb/ft³
Asian white birchBetula platyphylla1,007 lbf*38.8 lb/ft³
Downy birchBetula pubescens1,007 lbf*38.8 lb/ft³
Eastern hophornbeamOstrya virginiana1,658 lbf*48.9 lb/ft³
European alderAlnus glutinosa479 lbf*27.5 lb/ft³
European hornbeamCarpinus betulus1,658 lbf*48.9 lb/ft³
Gray alderAlnus incana479 lbf*27.5 lb/ft³
Gray birchBetula populifolia753 lbf*33.9 lb/ft³
Green alderAlnus viridis479 lbf*27.5 lb/ft³
Hazel alderAlnus serrulata479 lbf*27.5 lb/ft³
Himalayan birchBetula utilis1,007 lbf*38.8 lb/ft³
Italian alderAlnus cordata479 lbf*27.5 lb/ft³
Japanese hornbeamCarpinus japonica1,309 lbf*43.8 lb/ft³
Knowlton's hophornbeamOstrya knowltonii1,658 lbf*48.9 lb/ft³
Nepal alderAlnus nepalensis608 lbf*30.7 lb/ft³
Paper birchBetula papyrifera910 lbf38.5 lb/ft³
Red alderAlnus rubra590 lbf28.7 lb/ft³
River birchBetula nigra915 lbf*37.1 lb/ft³
Silver birchBetula pendula1,203 lbf*42.1 lb/ft³
Sweet birchBetula lenta1,470 lbf45.4 lb/ft³
Turkish hazelnutCorylus colurna1,203 lbf*42.1 lb/ft³
Virginia roundleaf birchBetula uber1,007 lbf*38.8 lb/ft³
Water birchBetula occidentalis1,007 lbf*38.8 lb/ft³
White alderAlnus rhombifolia479 lbf*27.5 lb/ft³
Yellow birchBetula alleghaniensis1,260 lbf43.3 lb/ft³