Wood Record

family

Bignoniaceae

The family Bignoniaceae supplies 27 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

7 of 27 carry a published Janka test.

WoodJankaDensity
African tuliptreeSpathodea campanulata395 lbf*25.1 lb/ft³
Black calabashAmphitecna latifolia1,152 lbf*41.3 lb/ft³
Black pouiJacaranda mimosifolia1,054 lbf*39.6 lb/ft³
Candle treeParmentiera cereifera2,064 lbf*54.2 lb/ft³
Caroba / paraparáJacaranda copaia423 lbf26.0 lb/ft³
Chinese catalpaCatalpa ovata509 lbf*28.2 lb/ft³
Common calabash treeCrescentia cujete1,103 lbf*40.5 lb/ft³
CuachiloteParmentiera aculeata1,923 lbf*52.4 lb/ft³
Desert willowChilopsis linearis915 lbf*37.1 lb/ft³
Haitian catalpaCatalpa longissima1,007 lbf*38.8 lb/ft³
Houka, calabashCrescentia alata1,419 lbf*45.5 lb/ft³
IpeTabebuia spp., lapacho group3,680 lbf70.0 lb/ft³
IpêHandroanthus serratifolius = Tabebuia serratifolia3,100 lbf72.5 lb/ft³
IpêTabebuia sp1,280 lbf63.7 lb/ft³
Ipê-amareloHandroanthus incanus = Tabebuia cf incana3,147 lbf*65.5 lb/ft³
Kigelia africanaKigelia africana1,203 lbf*42.1 lb/ft³
Northern catalpaCatalpa speciosa509 lbf*28.2 lb/ft³
Peroba de camposParatecoma peroba1,600 lbf46.0 lb/ft³
Pink tabebuiaTabebuia pallida1,054 lbf*39.6 lb/ft³
Pink trumpet-treeTabebuia rosea1,054 lbf*39.6 lb/ft³
PrimaveraTabebuia donnell–smithii660 lbf29.0 lb/ft³
RobeTabebuia spp., roble group960 lbf40.0 lb/ft³
Roble coloradoTabebuia schumanniana1,923 lbf*52.4 lb/ft³
RruDolichandrone spathacea509 lbf*28.2 lb/ft³
Southern catalpaCatalpa bignonioides509 lbf*28.2 lb/ft³
White cedarTabebuia heterophylla1,152 lbf*41.3 lb/ft³
Yellow trumpetbushTecoma stans915 lbf*37.1 lb/ft³