family
Boraginaceae
The family Boraginaceae supplies 20 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
6 of 20 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Anacahuita Texas OliveCordia boissieri | 1,203 lbf* | 42.1 lb/ft³ |
| Anacua knockawayEhretia anacua | 1,419 lbf* | 45.5 lb/ft³ |
| BodywoodBourreria succulenta | 1,852 lbf* | 51.5 lb/ft³ |
| CanaleteCordia spp. (hard-wooded, dark-colored Gerascanthus group) | 2,200 lbf | 58.2 lb/ft³ |
| Fragrant manjackCordia dichotoma | 451 lbf* | 26.7 lb/ft³ |
| Frei-jorgeCordia sp. | 960 lbf* | 40.0 lb/ft³ |
| FreijóCordia bicolor | 963 lbf | 37.1 lb/ft³ |
| FreijóCordia goeldiana | 996 lbf | 36.3 lb/ft³ |
| FreijóCordia sagotii | 882 lbf | 38.0 lb/ft³ |
| KouCordia subcordata | 875 lbf* | 36.3 lb/ft³ |
| Largeleaf geigertreeCordia sebestena | 1,309 lbf* | 43.8 lb/ft³ |
| Laurel BlancoCordia spp. (soft-wooded, light-colored Alliodora group) | 1,000 lbf | 37.0 lb/ft³ |
| Mucilage manjackCordia sulcata | 641 lbf* | 31.5 lb/ft³ |
| MunecoCordia borinquensis | 1,788 lbf* | 50.7 lb/ft³ |
| Red manjackCordia collococca | 915 lbf* | 37.1 lb/ft³ |
| Rochefortia spinosaRochefortia spinosa | 3,965 lbf* | 73.4 lb/ft³ |
| Spanish elmCordia alliodora | 915 lbf* | 37.1 lb/ft³ |
| TouCordia aspera | 509 lbf* | 28.2 lb/ft³ |
| West African CordiaCordia millenii | 590 lbf | 25.0 lb/ft³ |
| ZiricoteCordia dodecandra | 2,530 lbf* | 59.6 lb/ft³ |