family
Burseraceae
The family Burseraceae supplies 19 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
11 of 19 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| African CanaríumCanarium schweinfurthii | 670 lbf | 30.0 lb/ft³ |
| AmesclaTrattinnickia burserifolia | 697 lbf | 35.5 lb/ft³ |
| BarroteTetragastris panamensis | 2,693 lbf | 57.4 lb/ft³ |
| BreuProtium sp. | 2,317 lbf | 39.0 lb/ft³ |
| BreuProtium heptaphyllum | 877 lbf | 42.1 lb/ft³ |
| Breu-brancoDacryodes sp | 948 lbf | 36.8 lb/ft³ |
| Breu-mangaTetragastris altissima | 2,169 lbf | 58.7 lb/ft³ |
| Breu-pretoProtium tenuifolium | 1,517 lbf | 48.9 lb/ft³ |
| Canarium vulgareCanarium vulgare | 875 lbf* | 36.3 lb/ft³ |
| GommierDacryodes excelsa | 900 lbf | 40.0 lb/ft³ |
| Gumbo-LimboBursera simaruba | 395 lbf* | 25.1 lb/ft³ |
| Haplolobus floribundusHaplolobus floribundus | 1,725 lbf* | 49.9 lb/ft³ |
| KedondongCanarium spp. | 695 lbf* | 33.0 lb/ft³ |
| LukerrCanarium indicum | 1,103 lbf* | 40.5 lb/ft³ |
| MaaliCanarium vitiense | 915 lbf* | 37.1 lb/ft³ |
| Manuai vivaoGaruga floribunda | 1,309 lbf* | 43.8 lb/ft³ |
| MesecheuesCanarium hirsutum | 960 lbf* | 38.0 lb/ft³ |
| OkoumeAucoumea klaineana | 380 lbf | 28.0 lb/ft³ |
| SaliTetragastris spp. | 1,970 lbf | 54.0 lb/ft³ |