family
Caesalpiniaceae
The family Caesalpiniaceae supplies 22 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
21 of 22 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AngélicaDicorynia paraensis | 946 lbf | 36.2 lb/ft³ |
| ArapariMacrolobium acacifolium | 1,153 lbf | 39.3 lb/ft³ |
| ArarapariMacrolobium sp | 1,208 lbf | 40.0 lb/ft³ |
| CanafístulaCassia fastuosa | 2,500 lbf | 54.3 lb/ft³ |
| CopaíbaCopaifera sp. | 1,007 lbf | 37.5 lb/ft³ |
| CopaíbaCopaifera multijuga | 1,067 lbf | 39.3 lb/ft³ |
| CopaíbaCopaifera duckei | 1,464 lbf | 48.1 lb/ft³ |
| CopaíbaCopaifera reticulata | 1,464 lbf | 48.1 lb/ft³ |
| CourbarilHymenaea courbaril | 2,350 lbf | 56.0 lb/ft³ |
| JataipebaDialium guianense | 3,650 lbf | 63.7 lb/ft³ |
| Jatobá / jutaí-do-campoHymenaea parvifolia | 3,792 lbf | 73.4 lb/ft³ |
| MuirapixunaChamaecrista scleroxylon = Cassia scleroxylon | 3,435 lbf | 84.1 lb/ft³ |
| Pau-pongaTachigali sp. | 1,019 lbf | 36.2 lb/ft³ |
| Pinho-cuiabanoSchizolobium parahyba = Schizolobium amazonicum | 586 lbf | 29.3 lb/ft³ |
| RoxinhoParkia sp | 276 lbf* | 20.0 lb/ft³ |
| RoxinhoParkia pendula | 952 lbf | 38.4 lb/ft³ |
| TaxiTachigali glauca = Tachigali myrmecophila | 1,505 lbf | 43.4 lb/ft³ |
| Taxi-brancoTachigali cavipes | 818 lbf | 34.3 lb/ft³ |
| Taxi-pitombaTachigali chrysophylla =Sclerolobium chrysophyllum | 1,378 lbf | 47.7 lb/ft³ |
| Taxi-pitombaTachigali poeppigiana = Sclerolobium poeppigianum | 1,479 lbf | 50.7 lb/ft³ |
| Taxi-preto / taxiaranaTachigali paraensis = Sclerolobium paraense | 1,962 lbf | 47.3 lb/ft³ |
| Taxi-preto / ziquitaTachigali multijuga | 1,166 lbf | 40.0 lb/ft³ |